Stabilization/solidification of a municipal solid waste incineration residue using fly ash-based geopolymers
Abstract
The stabilization/solidification (S/S) of a municipal solid waste incineration (MSWI) fly ash containing hazardous metals such as Pb, Cd, Cr, Zn or Ba by means of geopolymerization technology is described in this paper. Different reagents such as sodium hydroxide, potassium hydroxide, sodium silicate, potassium silicate, kaolin, metakaolin and ground blast furnace slag have been used. Mixtures of MSWI waste with these kinds of geopolymeric materials and class F coal fly ash used as silica and alumina source have been processed to study the potential of geopolymers as waste immobilizing agents. To this end, the effects of curing conditions and composition have been tested. S'S solids are submitted to compressive strength and leaching tests to assess the results obtained and to evaluate the efficiency of the treatment. Compressive strength values in the range 1-9 MPa were easily obtained at 7 and 28 days. Concentrations of the metals leached from S/S products were strongly pH dependent, showing that the leachate pH was the most important variable for the immobilization of metals. Comparison of fly ash-based geopolymer systems with classical Portland cement stabilization methods has. also been accomplished. (C) 2010 Elsevier B.V. All rights reserved.
Más información
Título según WOS: | ID WOS:000289446700052 Not found in local WOS DB |
Título de la Revista: | JOURNAL OF HAZARDOUS MATERIALS |
Volumen: | 185 |
Número: | 1 |
Editorial: | Elsevier |
Fecha de publicación: | 2011 |
Página de inicio: | 373 |
Página final: | 381 |
DOI: |
10.1016/j.jhazmat.2010.08.127 |
Notas: | ISI |